Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 2.23e+11 ohm @Time 86400 sec |
2.23e+11 ohm @Time 24.0 hour |
Control; IPC B24 |
Indium Corp. 1075-EXR 30 VOC-Free Wave Solder Flux 1075-EXR 30 VOC-free, is a non-halide, synthetic resin flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075-EXR 30 VOC-Free is .. |