Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 100000 - 2.00e+7 ohm | 100000 - 2.00e+7 ohm | Average value: 4.44e+6 ohm Grade Count:10 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |