Polymer Property : Insulation Resistance = 1.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE
Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w..
Insulation Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
Lehmann & Voss LUVOCOM® 1105/GF/14 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f..
Insulation Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
Lehmann & Voss LUVOCOM® 1105-1963 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f..
Insulation Resistance 1.00e+14 ohm
1.00e+14 ohm
MIL-I-46058C
Aptek 7503LM-PMF UV Urethane Conformal Coating
UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p..
Insulation Resistance 1.00e+14 ohm
1.00e+14 ohm
MIL-I-46058C
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant
UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, ..