Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 9.76 kV/mm @Temperature 121 °C, Time 10800 sec |
248 kV/in @Temperature 250 °F, Time 3.00 hour |
0.0625 in. thickness; ASTM D149 |
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing Microcellular PTFE gasket with rigid PTFE coreHighly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flangesCompressible layers conform to surface irregularit.. |