Polymer Property : Dielectric Strength = 870 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 34.3 kV/mm

@Temperature 150 °C
870 kV/in

@Temperature 302 °F
ASTM D149-97A
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Dielectric Strength 34.3 kV/mm

@Temperature 150 °C
870 kV/in

@Temperature 302 °F
ASTM D149-97A
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Dielectric Strength 34.3 kV/mm

@Temperature 150 °C
870 kV/in

@Temperature 302 °F
ASTM D149-97A
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Dielectric Strength 34.3 kV/mm

@Temperature 150 °C
870 kV/in

@Temperature 302 °F
ASTM D149-97A
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..