Polymer Property : Dielectric Strength = 780 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 30.7 kV/mm

@Thickness 1.60 mm
780 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.