Dielectric Strength 73.11 kV/mm

@Thickness 0.356 mm,
Frequency 50.0 Hz
1857 kV/in

@Thickness 0.0140 in,
Frequency 50.0 Hz
continuously increasing at 500 V/sec, 6.3 mm electrodes
DuPont Teijin Films Melinex® 238 Polyester Film
Melinex® 238 is a translucent white polyester film used for electrical insulation. It has been specially developed for use as an electrical insulation material in rotating electrical machines. It i..