Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 62.0 kV/mm @Thickness 0.800 mm |
1570 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |