Polymer Property : Dielectric Strength = 478 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 553 PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific)
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 553U PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.