Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 44.0 kV/mm @Thickness 0.800 mm |
1120 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free.. |