Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.1 kV/mm @Thickness 3.20 mm |
409 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics ULTEM STM1500 PEI Copolymer Siloxane polyetherimide block copolymer. Wire and cable use. Strength and flexibility. |