Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.4 kV/mm @Frequency 60.0 Hz |
391 kV/in @Frequency 60.0 Hz |
step-by-step, dry; ASTM D149 |
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc. |