Electrical Properties Metric English Comments
Dielectric Strength 39.4 kV/mm

@Temperature 125 °C
1000 kV/in

@Temperature 257 °F
ASTM D149-97A
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Dielectric Strength 39.4 kV/mm

@Temperature 175 °C
1000 kV/in

@Temperature 347 °F
ASTM D149-97A
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Dielectric Strength 39.4 kV/mm

@Temperature 125 °C
1000 kV/in

@Temperature 257 °F
ASTM D149-97A
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Dielectric Strength 39.4 kV/mm

@Temperature 175 °C
1000 kV/in

@Temperature 347 °F
ASTM D149-97A
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Dielectric Strength 39.4 kV/mm

@Temperature 125 °C
1000 kV/in

@Temperature 257 °F
ASTM D149-97A
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Dielectric Strength 39.4 kV/mm

@Temperature 175 °C
1000 kV/in

@Temperature 347 °F
ASTM D149-97A
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..