Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 31.5 kV/mm @Thickness 1.57 mm |
800 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Dielectric Strength | 31.5 kV/mm @Thickness 1.57 mm |
800 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
Dielectric Strength | 31.5 kV/mm @Thickness 1.57 mm |
800 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |