Electrical Properties Metric English Comments
Dielectric Strength 3.40 kV/mm

@Frequency 60.0 Hz
86.4 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America SI 9041A Silicone Compound
SI 9041A is a long fiberglass reinforced silicone molding compound, which exhibits excellent high temperature properties in addition to good molding characteristics for transfer and compression mold..