Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 9.65 kV/mm @Temperature 121 °C, Time 10800 sec |
245 kV/in @Temperature 250 °F, Time 3.00 hour |
0.125 in. thickness; ASTM D149 |
Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sea.. |