Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.9 kV/mm @Thickness 1.60 mm, Temperature 23.0 °C |
556 kV/in @Thickness 0.0630 in, Temperature 73.4 °F |
500 V/s in oil; ASTM D149 |
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc.. |
|||
Dielectric Strength | 21.9 kV/mm @Thickness 3.20 mm |
556 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific) 40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif.. |