Polymer Property : Dielectric Strength = 19.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 19.3 kV/mm

@Thickness 1.02 mm
490 kV/in

@Thickness 0.0400 in
ASTM-D149
CoorsTek ADS-96R 96% Alumina Thick Film Substrate
This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers