Polymer Property : Dielectric Strength = 18.1 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM CRS5011R PEI
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM UF5011S PEI
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Dielectric Strength 18.1 kV/mm

@Thickness 3.20 mm
460 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Dielectric Strength 18.1 kV/mm

@Thickness 1.57 mm
460 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP321 Cotton Fabric  (discontinued **)
Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f..