Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 102 kV/mm @Thickness 0.0508 mm |
2580 kV/in @Thickness 0.00200 in |
Z Direction; IPC-TM-650 2.5.6.2 |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |
|||
Dielectric Strength | 102 kV/mm @Temperature 125 °C |
2600 kV/in @Temperature 257 °F |
ASTM D149-97A |
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Dielectric Strength | 102 kV/mm @Temperature 125 °C |
2600 kV/in @Temperature 257 °F |
ASTM D149-97A |
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Dielectric Strength | 102 kV/mm @Temperature 125 °C |
2600 kV/in @Temperature 257 °F |
ASTM D149-97A |
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |