Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.4 kV/mm @Thickness 3.17 mm |
264 kV/in @Thickness 0.125 in |
100% RH for 96 hours; ASTM D149 |
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing Microcellular PTFE gasket with rigid PTFE coreHighly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flangesCompressible layers conform to surface irregularit.. |