Polymer Property : Shielding Effectiveness = 59 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 59 dB
59 dB
ASTM D4935
Techmer ES Electrablend® PC NCF15 FR 15% Nickel-Coated Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation ..