Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 98 dB @Frequency 4.00e+8 Hz |
98 dB @Frequency 4.00e+8 Hz |
P-Field |
P & P Technology Monel-BS3075 (NA13) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | 98 dB @Frequency 1.00e+8 Hz |
98 dB @Frequency 1.00e+8 Hz |
5mm x 25.4mm |
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec.. |