Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 89 dB @Frequency 1.00e+10 Hz |
89 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® FR750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 89 dB @Frequency 1.00e+10 Hz |
89 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® 864 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |