Polymer Property : Shielding Effectiveness = 71 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 71 dB

@Frequency 2.00e+8 Hz
71 dB

@Frequency 2.00e+8 Hz
CHO-TP08
Parker Chomerics CHO-FORM 5531 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed..