Electrical Properties Metric English Comments
Shielding Effectiveness 64 dB

@Frequency 1.00e+8 Hz
64 dB

@Frequency 1.00e+8 Hz
ASTM D4935
Parker Chomerics PREMIERâ„¢ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..