Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 63 dB @Frequency 1.00e+9 Hz |
63 dB @Frequency 1.00e+9 Hz |
|
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C.. |