Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 49 dB @Frequency 100000 Hz |
49 dB @Frequency 100000 Hz |
H-Field |
P & P Technology Monel-BS3075 (NA13) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | 49 dB @Frequency 4.00e+8 Hz |
49 dB @Frequency 4.00e+8 Hz |
360° Ground Termination |
Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight .. |