Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 107 dB

@Frequency 1.00e+7 Hz
107 dB

@Frequency 1.00e+7 Hz
E-Field, Electrical
P & P Technology BS3075 NA13 Monel Wire
Alloy 400L Wire Diameter 0.11mmInformation provided by P & P Technology
Shielding Effectiveness 107 dB

@Frequency 1.00e+10 Hz
107 dB

@Frequency 1.00e+10 Hz
P-Field
P & P Technology Conductive Elastomer
Nickel Graphite particlesInformation provided by P & P Technology
Shielding Effectiveness 107 dB

@Frequency 1.00e+9 Hz
107 dB

@Frequency 1.00e+9 Hz
3mm x 25.4mm
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket
Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec..