Polymer Property : Shielding Effectiveness = 103 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 103 dB

@Frequency 1.00e+9 Hz
103 dB

@Frequency 1.00e+9 Hz
Parker Chomerics SOFT-SHIELD® 5000 Low Closure Force EMI Gasket
Description: SOFT-SHIELD® 5000 Series EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electron..
Shielding Effectiveness 103 dB

@Frequency 1.00e+10 Hz
103 dB

@Frequency 1.00e+10 Hz
1.5mm x 25.4mm
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket
Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec..
Shielding Effectiveness 103 dB

@Frequency 1.00e+9 Hz
103 dB

@Frequency 1.00e+9 Hz
5mm x 25.4mm
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket
Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec..