Polymer Property : Shielding Effectiveness = 0.60 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness >= 0.60 dB

@Frequency 4.00e+10 Hz
>= 0.60 dB

@Frequency 4.00e+10 Hz
Plane Wave; Method 1, CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i..