Electrical Properties Metric English Comments
Shielding Effectiveness -15.0 dB

@Thickness 1.57 mm,
Frequency 9.80e+9 Hz
-15.0 dB

@Thickness 0.0620 in,
Frequency 9.80e+9 Hz
NRL Arch Test Method
Parker Chomerics CHO-MUTE 9020 RF Absorber
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone..
Shielding Effectiveness -15.0 dB

@Thickness 1.57 mm,
Frequency 1.05e+10 Hz
-15.0 dB

@Thickness 0.0620 in,
Frequency 1.05e+10 Hz
Microwave Absorption
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon..
Shielding Effectiveness -15.0 dB

@Thickness 1.57 mm,
Frequency 9.80e+9 Hz
-15.0 dB

@Thickness 0.0620 in,
Frequency 9.80e+9 Hz
Microwave Absorption
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon..