Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 90.0 - 127 sec | 90.0 - 127 sec | Average value: 116 sec Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Arc Resistance | 90.0 - 123 sec | 90.0 - 123 sec | Average value: 98.3 sec Grade Count:6 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |