Polymer Property : Arc Resistance = 85.0 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 40.0 - 85.0 sec
40.0 - 85.0 sec
Average value: 66.7 sec Grade Count:3
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Arc Resistance 80.0 - 85.0 sec
80.0 - 85.0 sec
Average value: 82.3 sec Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..