Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 67.0 - 135 sec | 67.0 - 135 sec | Average value: 107 sec Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |