Polymer Property : Arc Resistance = 345 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 345 sec
345 sec
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite
Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m..