Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 314 sec | 314 sec | ASTM D495 |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |