Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 292 sec | 292 sec | |
Pyrotek ISOMAG® 175 Structural Insulation Board Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr.. |