Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 220 sec | 220 sec | ASTM D495 |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Arc Resistance | 220 sec | 220 sec | ASTM D495-61 |
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm.. |