Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 205 sec | 205 sec | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |