Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 199 sec | 199 sec | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |