Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 137 - 188 sec | 137 - 188 sec | Average value: 168 sec Grade Count:24 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Arc Resistance | 115 - 188 sec | 115 - 188 sec | Average value: 172 sec Grade Count:14 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |