Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 17 sec @Thickness 3.17 mm |
17 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP101 Synthetic Fabric Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp.. |