Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 153 sec | 153 sec | ASTM D495 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Arc Resistance | 153 sec | 153 sec | ASTM D495 |
Plenco 6527 Phenolic, Granular, Injection Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |