Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 129 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 129 sec
129 sec
ASTM D495
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap..
Arc Resistance 129 sec
129 sec
ASTM D495
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Arc Resistance 129 sec
129 sec
ASTM D495
Celanese IMPET 340R PET, 45% Glass Reinforced
Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.I..
Arc Resistance 129 sec
129 sec
ASTM D495
Celanese Impet® 330 30% Glass-Reinforced Injection Moldable PET Polyester
Description: Impet 330 is a 30% glass-reinforced injection moldable PET polyester. It provides an excellent combination of strength, stiffness, and high temperature resistance.Information provided b..
Arc Resistance 129 sec
129 sec
ASTM D495
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Arc Resistance 129 sec
129 sec
ASTM D495
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Arc Resistance 129 sec
129 sec
IPC-TM-650.2.5.1
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy
The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW..
Arc Resistance 129 sec
129 sec
ASTM D495
Celanese Impet® 340R PET, 45% Glass Reinforced  (Unverified Data**)
Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.4..