Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 126 sec | 126 sec | ASTM D495 |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 126 sec | 126 sec | ASTM D495 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc. |
|||
Arc Resistance | 126 sec | 126 sec | ASTM D495 |
Plenco 2535 Phenolic, Granular, Injection Molded PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c.. |
|||
Arc Resistance | 126 sec | 126 sec | ASTM D495 |
Toyobo Vylopet® EMC415 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: accessory componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high di.. |
|||
Arc Resistance | 126 sec | 126 sec | |
Dow Corning 7 RELEASE COMPOUND Silicone-based compound, light consistencyInformation provided by Dow Corning |
|||
Arc Resistance | 126 sec | 126 sec | IPC TM-650 2.5.1 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |