Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 101 - 126 sec | 101 - 126 sec | Average value: 120 sec Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |