Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+6 - 9.00e+9 ohm | 1.00e+6 - 9.00e+9 ohm | ASTM D257 |
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black Data provided by Clariant Masterbatches |
|||
Surface Resistivity per Square | 1.00e+6 - 9.00e+9 ohm | 1.00e+6 - 9.00e+9 ohm | ASTM D257 |
Clariant Renol PA2SP0023 Nylon 6, Impact and Flow Modified, ESD Protection Data provided by Clariant Masterbatches |