Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 80 ohm | 80 ohm | Printed through 230 stainless steel mesh with 13 micron emulsion |
Gwent Electronic Materials C2110309D5 Carbon Graphite Ink This is designed for screen-printing of working electrodes for electrochemical sensors. The paste is formulated to give superior printing properties with good definition for fine line printing.Produ.. |
|||
Surface Resistivity per Square | 80 ohm | 80 ohm | |
Gwent Electronic Materials F2071018D1 Transparent ITO Coated Film This polyester film is produced by vacuum sputter deposition of indium tin oxide (ITO), this process provides excellent adhesion and uniform coating.Used in components of touch screens and other pos.. |