Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 7.00e+15 ohm | 7.00e+15 ohm | GB/T1410-2006 |
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Surface Resistivity per Square | 7.00e+15 ohm | 7.00e+15 ohm | GB/T1410-2006 |
Sichuan Deyang Haton® hGR40DL Polyphenylene Sulfide, Glass Fiber Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |